Use of Titanium Grade 4 (UNS R50700) is not permitted for use in PV applications per ASME VIII-1 as it is not included on Table UNF 23.4
Any idea why? Any code cases available that permit its use at all?
I have looked at a lot of places and just cannot figure out the reason it is excluded and I seek your help.
Thanks!
 
It has limited ductility.
If you need strength look at Gr9.

= = = = = = = = = = = = = = = = = = = =
Plymouth Tube
 
But the specified min elongation requirements for Grade 4 and Grade 9 in Section II-B are the same (15%) [II-B for SB265]
 
There are many reason why material is not permitted for use in Codes and Standards;

forming problems
low ductility
embrittlement
weldability
lack of use or interest
 
The diff is that gr4 will just make 15% and gr9 is usually 25%.
Weldability and forming are also issues.

= = = = = = = = = = = = = = = = = = = =
Plymouth Tube
 
Thanks all for your help.
It seems I will need to look at alternatives to using gr 4.
 
ME321,

See also Code Case 2497 that permits some titanium alloys, it may help you in alternatives.

Nasir
Welding Engineer
DESCON ENGINEERING LIMITED
PAKISTAN
 
Thanks Fizza453
 