JasonLouie
Materials
I have a weld procedure with a consumable insert. The PQR reported the filler metal thickness for the insert at 1/8" and then ER316L filler metal thickness at 3/16".
The consumable insert and the fill/cap pass filler metal have the same F-No. and A-No. (316L). The WPS does not distinguish between the two and just states that it is qualified for 316L filler metal to a maximum of 5/8".
Since SFA number nor the use of consumable inserts are not essential variables, are they qualified to weld without a consumable insert for 5/8" in thickness?
I appreciate any help you can provide! Thanks!
The consumable insert and the fill/cap pass filler metal have the same F-No. and A-No. (316L). The WPS does not distinguish between the two and just states that it is qualified for 316L filler metal to a maximum of 5/8".
Since SFA number nor the use of consumable inserts are not essential variables, are they qualified to weld without a consumable insert for 5/8" in thickness?