Eng-Tips is the largest forum for Engineering Professionals on the Internet.

Members share and learn making Eng-Tips Forums the best source of engineering information on the Internet!

  • Congratulations dmapguru on being selected by the Eng-Tips community for having the most helpful posts in the forums last week. Way to Go!

Use of cathodic protection (sacrificial anodes) with Cast Iron (EN-GJL-250) in ph5 submerged medium?

Status
Not open for further replies.

Arshad Ahamed

Mechanical
Joined
Jul 31, 2018
Messages
23
Location
US
Greetings,

I have a customer who is to install cast-iron pump (en-gjl-250) submerged in medium (textile effluent) with pH5. Is installing sacrificial anodes a good measure to reduce corrosion rate and enhance pump life?

Medium temp : 40deg C.
ph : 5


Be curious, and furious in your pursuit for answers
 
Did anyone do the math on the anodes?
At that pH they will be consumed quickly.
They will need to check often.

= = = = = = = = = = = = = = = = = = = =
P.E. Metallurgy, consulting work welcomed
 