We have a horizontal centrifual pump in a raw (lake) water system. We are apparently considering the use of a Belzona product to coat the inside of the pump casing to protect it from erosion/corrosion. Since this is a critical-application pump, should I be concerned about the Belzona coating chipping or flaking off at some point and locking the impeller? Unfortunately, I don't have any more specific details at this point, and I have not talked to Belzona yet, although I intend to when I get the chance. I was just looking for any opinions or operating experience you folks might have. I've seen Belzona used on piping and valve seats before, but not pump casings.