Continue to Site

Eng-Tips is the largest engineering community on the Internet

Intelligent Work Forums for Engineering Professionals

  • Congratulations cowski on being selected by the Eng-Tips community for having the most helpful posts in the forums last week. Way to Go!

urea production

Status
Not open for further replies.

bastean

Agricultural
Mar 4, 2008
4
Urea is produced with ammonia and carbon dioxide. Could the C02 from burning coal be dealt with through urea production for fertilizer?
 
Replies continue below

Recommended for you

CO2 is CO2. The only issue is the cost.

The problem is that the Urea process is a high pressure process. This would require recovering high purity CO2 from the flue gas and then compressing it.

The plant I worked at recovered the CO2 from an hydrogen reformer and then later as liquid CO2 from an outside vendor.

--Mike--
 
CO2 is a by-product of ammonia production. that is why you see urea plants paired with ammonia plants.
 