CO2 is CO2. The only issue is the cost.
The problem is that the Urea process is a high pressure process. This would require recovering high purity CO2 from the flue gas and then compressing it.
The plant I worked at recovered the CO2 from an hydrogen reformer and then later as liquid CO2 from an outside vendor.