UNS C72420 / Marinel /Nibron Special. Where to get in US?

Status
Not open for further replies.

metootoo

Mechanical
Joined
Aug 9, 2007
Messages
21
Location
US
I often have problems with getting products made in the US that were designed in the UK? Machine shops are always asking for substitute materials. I prefer to use what's specified whenever possible.

In this case UNS C72420. Where can I get it from? If no where in the US, then what high strength bronze can I replace it with? I need it's 80ksi minimum tensile strength, its level of corrosion resistance, and resistance to gall against 17-4 stainless.

Any help would be appreciated.
 
I also need the hardness of 220-320 HB
 
You may need to purchase material from the UK sources and supply it to your machine shops.

I don't know of a US producer, maybe you can find a specialty distributor that handles it.

= = = = = = = = = = = = = = = = = = = =
Plymouth Tube
 