Unloading a torque wrench - spring weakening.

Status
Not open for further replies.

johnSchwaner

Aerospace
Jan 15, 2007
41
It has been the common recommendation to return a snap style torque wrench to its lowest setting after usage. The often given reason is that the spring, if left compressed, will weaken.

I have always questioned the reason (not the practice). Will the spring weaken (creep) under sustained loading?

ps Hope this is a valid spring question!
 
Replies continue below

Recommended for you

Creep is real.
Some springs more than others, but they all do it.



Mike Halloran
Pembroke Pines, FL, USA
 
I believe The exact term is relaxation. Creep is under constant load while relaxation is under constant deflection.
 
Thank you for your responses. I was able to do a google search on spring relaxation to further my knowledge.
 