Hello all,

I have some unknown scrap material and the documentation that comes with it, identity the scrap with the following composition:

Fe 86%
Sre 0.44%
BrO 0.02%
La 0.68%
Ai 0.94%
SiO2 0.5%
CaO 0.5%
Cr 2.12%
Mn 0.4%
C Co 0.25%
Pd/Sr iba 5%

Does anybody knows what is it? Some scrap dealers says that it can be made into magnets but they are not very sure.

Thank you.

Koeskoes
 