May 4, 2020 #1 edward995 Industrial Joined May 4, 2020 Messages 9 Location MY why there is a line on the round bar? https://files.engineering.com/getfile.aspx?folder=ad0bb1c7-1caa-43e8-95da-9382c28f57a1&file=0fb37696-40e7-4fbc-be6f-24b8aecf9b16.jpg
May 5, 2020 #2 EdStainless Materials Joined May 20, 2004 Messages 16,356 Location Waukesha WI USA This looks to be hot finished bar. That line is from the hot rolling tooling. Have you tried to grind or turn a sample to see if it has depth? I doubt that it is a lapp or seam. = = = = = = = = = = = = = = = = = = = = P.E. Metallurgy Upvote 0 Downvote
This looks to be hot finished bar. That line is from the hot rolling tooling. Have you tried to grind or turn a sample to see if it has depth? I doubt that it is a lapp or seam. = = = = = = = = = = = = = = = = = = = = P.E. Metallurgy
May 5, 2020 #3 weldstan Materials Joined Jun 24, 2011 Messages 2,806 Location US Agree with Ed. Upvote 0 Downvote
May 5, 2020 #4 Guest Ditto. Not much to see here. "Everyone is entitled to their own opinions, but they are not entitled to their own facts." Upvote 0 Downvote
Ditto. Not much to see here. "Everyone is entitled to their own opinions, but they are not entitled to their own facts."