I have been given a sample of what initially looked like a Aluminium Nickel bronze, chemical analysis revealed a composition I could not find a standard for and was wondering if anyone has heard of an alloy with a composition similar to this:
Cu 60
Ni 15
Al 12
Zn 9
Si 1.5
Fe 1.2
also traces of Cl, Mn, As, Ga, Sn, Se, Cr, Pb
The nickel content seemed a little high for most Aluminium Nickel bronzes.
The sample in question has failed in both an inter and transgranular brittle manner.
Any help or suggestions greatly appreciated
Thanks
Gareth
I have been given a sample of what initially looked like a Aluminium Nickel bronze, chemical analysis revealed a composition I could not find a standard for and was wondering if anyone has heard of an alloy with a composition similar to this:
Cu 60
Ni 15
Al 12
Zn 9
Si 1.5
Fe 1.2
also traces of Cl, Mn, As, Ga, Sn, Se, Cr, Pb
The nickel content seemed a little high for most Aluminium Nickel bronzes.
The sample in question has failed in both an inter and transgranular brittle manner.
Any help or suggestions greatly appreciated
Thanks
Gareth