Dear experts !! I have the following situation: I have a fine coal silicon manufactured according to ASME VIII Div.1, the engineering requests the welds with ultrasound testing, to be only 20% of the welded length, however, the drawing says 100%. I ask: Is this allowed by ASME VIII Div.1? What part of the code tells me this?
Thank you in advance.
 
Replies continue below

Recommended for you

IS.13287 N1 said:
Is this allowed by ASME VIII Div.1?
- Yes

What part of the code tells me this?
- In general if it is not prohbiited, it is permitted.

Regards,

Mike


The problem with sloppy work is that the supply FAR EXCEEDS the demand
 
Glad to be of service :)

The problem with sloppy work is that the supply FAR EXCEEDS the demand
 
Status
Not open for further replies.

Part and Inventory Search

Sponsor