iLiConsult
Civil/Environmental
We are currently sounding concrete with a swiss-made ultrasonic instrument call TICO. Literature says that the pulse velocity for indirect or surface transmissio is 5 to 20% lower than the velocity of direct transmission.
In our tests we find the pulse velocity of indirect transmission 50 to 100% lower than the one for direct transmission.
Is anybody out there with experience in ultrasonic concrete testing?
In our tests we find the pulse velocity of indirect transmission 50 to 100% lower than the one for direct transmission.
Is anybody out there with experience in ultrasonic concrete testing?