Folks...
Recently encountered a unique part:
1.2500-Dia Threaded stud. It has precision ground shank ~1.5-long with 1.25-long threads on both ends [~4.0-L ttl]... made from 4340M [4340VAR] steel HT270--300-KSI FTu [~170-KSI FSu] with Cd-Ti alloy plating. The aerospace quality threads were specified as ROLLED.
The stud is used in a critical shear joint on a unique acft.
Not surprisingly a few of these studs have failed thru the threads due to hydrogen embrittlement.
Now I have seen/used 260-KSI steel, 300M, MP35 and MP159 bolts [or parts with threads]... but 4340M 270+-KSI fasteners were beyond my threshold od sanity.
Anyone else know-of steel alloy 270+-KSI fasteners in use.... or for that matter "any-alloy" 270+-KSI HT fastener-items [bolts, pins, studs, etc] in service?
This part is very scary to me...
Regards, Wil Taylor
Trust - But Verify!
We believe to be true what we prefer to be true.
For those who believe, no proof is required; for those who cannot believe, no proof is possible.
Recently encountered a unique part:
1.2500-Dia Threaded stud. It has precision ground shank ~1.5-long with 1.25-long threads on both ends [~4.0-L ttl]... made from 4340M [4340VAR] steel HT270--300-KSI FTu [~170-KSI FSu] with Cd-Ti alloy plating. The aerospace quality threads were specified as ROLLED.
The stud is used in a critical shear joint on a unique acft.
Not surprisingly a few of these studs have failed thru the threads due to hydrogen embrittlement.
Now I have seen/used 260-KSI steel, 300M, MP35 and MP159 bolts [or parts with threads]... but 4340M 270+-KSI fasteners were beyond my threshold od sanity.
Anyone else know-of steel alloy 270+-KSI fasteners in use.... or for that matter "any-alloy" 270+-KSI HT fastener-items [bolts, pins, studs, etc] in service?
This part is very scary to me...
Regards, Wil Taylor
Trust - But Verify!
We believe to be true what we prefer to be true.
For those who believe, no proof is required; for those who cannot believe, no proof is possible.