ChiangJaron
Industrial
All expert,
UCS-79(d)(5) specified rule "The temperature of the material during forming is
in the range of 250°F to 900°F (120°C to 480°C)."
Why the rule shecified a temperature range, not a limit temperature ?
If the head form is formed belowing 119°C, could I exempt the heat treatment based on this rule ?
UCS-79(d)(5) specified rule "The temperature of the material during forming is
in the range of 250°F to 900°F (120°C to 480°C)."
Why the rule shecified a temperature range, not a limit temperature ?
If the head form is formed belowing 119°C, could I exempt the heat treatment based on this rule ?