maryam1979;
Normally, I recommend posters to review the applicable section of the ASME Code, Section VIII, Div 1 UCS. I presume that you have done this, so I will attempt to answer your question;
1. Figure UCS is a diagram generated for impact exemption curves based on material thickness and minimum design metal temperature (MDMT). If your material of construction lies on or above the curve, impact testing is not required for the applicable minimum design metal temperature (MDMT) shown on the left axis. So, for example, material that would lie on Curve A, in Figure UCS-66, for thickness 0.394" or less, impact testing is not required for a minimum design metal temperature of 19 deg F or higher. As the thickness increases, the MDMT increases because of the effects of plane strain (or triaxial stresses).
2. It all depends on your selection of MDMT.