I am looking over a proposal for our company regarding a pressure vessel. The customer is stating that A516 Gr.70 does not need to be Charpy tested with a thickness less than 25mm for a design temperature of -50°C. I look at VIII Fig. UCS-66M and the lowest that A516 Gr.70 goes is to curve B, indicating -29°C. A516 Gr.70N (N = normalized) plate will fall under curve D indicating a -48°C design temperature.
Can anybody inform me if I am missing some part of code that allows plate to be used at -50°C without Charpy testing? The plate technically is going to be subjected to about 2 psi(g) because it is used more for casing around a pressure part.