I am investigating a case dating back to 2002. A number of 280mm outside diameter UPVC pipes where installed for water supply. The stamp on the outside of the pipe said DIN 19532.
I am finding it hard to get any information on this standard.
Is this DIN standard still in use?
What british standard could I use to check the specifications?
I need to measure the pipe to make sure that it was manufactured to the correct tolerances.

Any help would be much appreciated.

Regards,
Conor
 
I noticed noone had yet responded to you inquiry. I am not familiar with the specific standard you are referring to, but I was just curious where exactly the "280 mm" you stated comes from (is this actually written on the pipe or a nominal O.D. dimension from a table you are looking at from this referenced standard, or is this one actual O.D. measurement as from a "pi" tape etc)?

[It is some interesting this dimension is only very slightly less than the 11.10 inch nominal outside diameter of nominal ten inch AWWA ductile iron or pvc pipe.]
 
I went to my IHS subscription and found out that DIN is a German Standard (DIN - Deutsches Institut Fur Normung E.V.). There does not seem to be a standard 19532, but that could just be that I'm not searching correctly.

Patricia Lougheed

Please see FAQ731-376: Eng-Tips.com Forum Policies for tips on how to make the best use of the Eng-Tips Forums.
 
The most common European standard is

ISO 15493 Plastics piping systems for industrial
applications — Acrylonitrile-butadienestyrene
(ABS), unplasticized poly(vinyl
chloride) (PVC-U) and chlorinated
poly(vinyl chloride) (PVC-C) —
Specifications for components and the
system ? Metric series

No DIN standards are referenced therein

Suggest you contact the manufacturer and seek a copy from them.

Rconner,

280mm is a common PVC-U size and refers to the OD. It is used with DN250 DI fittings.

 
I found the standard it states that the piping tolerance should be +0.6mm -0.00mm does this sound correct, I thought that the tolerance would allow both in the + and - dimensions i.e +0.6mm -0.6mm.
 
stanier, thanks for the education (incidentally, am also curious what is the standard for the specific "DN250 DI fittings" you are talking about, and the specific dimension/tolerance pvc to DI joining design you are referring to?)
 
rconner,

Australian Standard AS 2280-2004 Ductile Iron pipe & Fittings. Dimensions are perhaps peculiar to this market downunder.

The PVC manufacturers (Vinidex and Iplex pipelines) here produce pipe to match the size of ductile iron. PVC-U, PVC-M and PVC-O are extruded.

 
gradeng84 said:
I found the standard it states that the piping tolerance should be +0.6mm -0.00mm does this sound correct, I thought that the tolerance would allow both in the + and - dimensions i.e +0.6mm -0.6mm.

There are quite a few standards that give tolerances in one direction only. The best bet would be to contact DIN.

Patricia Lougheed