What would be appropriate for the concrete used in a small town wastewater treatment plant for the tanks set in the ground. The town is in a region that gets winters to -10 deg. F and snow and summers to 100 deg. F (i.e. Midwest US). This is a very small town.
Studying ACI 350 I get the following:
Types I thru V cements can be used.
Question: Is type II or V preferable?
Use largest practical aggregate.
Use air entrainment.
Use fly ash.