PatCouture
Mechanical
Hi, I'm sorry for my lack of knowledge on the subject, but I would like to use a block of aluminium to build a little machine, I want aluminium that has good machinability properties and will be used in a corrosive environment (food processing). I don't know much about this material maybe I simply need the most common type of aluminium but I don't know what's the right number.
Thanks in advance
Patrick