Apr 2, 2008 #1 qcben Industrial Joined Jul 20, 2007 Messages 3 Location CA Can a single sided, V-groove butt joint without backing be considered a type 1 weld as per ASME VIII Div. 1 UW-12? This weld would have a GMAW root and SAW fill and cap.
Can a single sided, V-groove butt joint without backing be considered a type 1 weld as per ASME VIII Div. 1 UW-12? This weld would have a GMAW root and SAW fill and cap.
Apr 2, 2008 #2 JoeTank Structural Joined Oct 28, 1999 Messages 1,133 Location US Yes, but only if the backside of the weld can be visually eaxmined to verify Code compliance for undercut, weld profile and reinforcement. Joe Tank Upvote 0 Downvote
Yes, but only if the backside of the weld can be visually eaxmined to verify Code compliance for undercut, weld profile and reinforcement. Joe Tank
Apr 14, 2008 #3 moseley Chemical Joined Feb 4, 2002 Messages 65 Location US You also need to follow the limitations set forth by Table UW-12. Upvote 0 Downvote