Does any one have the TYE of 6063-T832 drawn tube? I had a link in my favorites of a materials .org site that had pretty much everything it was like mtls.org but lost it. If some one can give me the info or the site or both, Id be greatful thanks.

Joe
 
My Aluminum Association book shows UTS of 41ksi min; TYS of 36ksi min and %E of 5 min. This is for wall thickness up to .049". For heavier wall, UTS &TYS drop by 1ksi.
 