Continue to Site

Eng-Tips is the largest engineering community on the Internet

Intelligent Work Forums for Engineering Professionals

  • Congratulations waross on being selected by the Eng-Tips community for having the most helpful posts in the forums last week. Way to Go!

TYE of 6063-T832??

Status
Not open for further replies.

NorthJ

Mechanical
Jun 14, 2005
13
Does any one have the TYE of 6063-T832 drawn tube? I had a link in my favorites of a materials .org site that had pretty much everything it was like mtls.org but lost it. If some one can give me the info or the site or both, Id be greatful thanks.

Joe
 
Replies continue below

Recommended for you

My Aluminum Association book shows UTS of 41ksi min; TYS of 36ksi min and %E of 5 min. This is for wall thickness up to .049". For heavier wall, UTS &TYS drop by 1ksi.
 