Hi Stan000,
A separate PQR is required to qualify welding procedures to weld up to 1" thick.Frst of all the combinations of the qulaifed PQR's do not add uo to weld 1" thick base metal. Also the shielding gases are different warranting a new PQR to be qualified, refer QW 408(C).
To come back to the point of Duplex welding:
[ul]
[li][/li]
[/ul]It requires a careful and through evaluation and planning prior to welding of any procedure or production welds.
Pleanty of resoureces are available as guidence for welding DSS, however thourough understanding of metalliurgy and welding processes are required to get the due success.
Thanks.
Pradip Goswami,P.Eng.IWE
Welding & Metallurgical Specialist
Ontario,Canada.