fortmceng
Mechanical
- Nov 16, 2008
- 18
I am looking for some information on Stress Relieving requirements of Carbon Steel Tubes U Bends for Heat Exchanger (Material: SA179, Code API 660, ASME Sec VIII D1):
API 660 is not very clear and leaves it for the customer to decide. What should be the best approach in the absence of clear guidelines from code.
1) Is Electric Resistant method acceptable.
2) What should be the cooling and heating rate.
3) How much hold time should be sufficient.
The intent is to relieve residual stresses due to cold forming. I have come across some manufacturer's who thinks ER is sufficient whereas others prefer Furnace method for SR. There is substantial difference in cost between these two methods. I would like to know what should be the basis for selecting SR methods. Application is in a refinery.
Thanks in advance.