There is a 4 tube pass/1 shell pass heat exchanger experiencing failure (leaks) at some especific middle tubes of the 1st pass (6 tubes out of 125 total in the 1st pass). Localized corrosion seems to be taking place on the tubes outside, toward the floating head. Process conditions / are:
Tube Side: Diesel, in: 600 F, out 395-400 F, Total sulfur = 3 ppm ,
Shell Side: Gasoil, in: 200 F, out 300 F, total sulfur = 2.6 w %
Total number of tubes=500 (125 each of the 4 pass). Tube lenght: 6 mts. Material: CS (SA 179)
Temperature profiles gotten from process simulation are lower than 410 - 420 F near the location where the tubes have being found holed (at 5 mts from the inlet or 1 mts from the floating head end), on the contrary where the predicted tube wall temperature is higher (towards the fixed tubesheet end), no significant corrosion/metal loss is found.
I would appreciate if this comunity might provide some insights on the causes of these tubes failures. Thanks!
Tube Side: Diesel, in: 600 F, out 395-400 F, Total sulfur = 3 ppm ,
Shell Side: Gasoil, in: 200 F, out 300 F, total sulfur = 2.6 w %
Total number of tubes=500 (125 each of the 4 pass). Tube lenght: 6 mts. Material: CS (SA 179)
Temperature profiles gotten from process simulation are lower than 410 - 420 F near the location where the tubes have being found holed (at 5 mts from the inlet or 1 mts from the floating head end), on the contrary where the predicted tube wall temperature is higher (towards the fixed tubesheet end), no significant corrosion/metal loss is found.
I would appreciate if this comunity might provide some insights on the causes of these tubes failures. Thanks!