TSA coating breakdown factor !! 1

Status
Not open for further replies.

hsemus

Petroleum
Apr 26, 2012
42
I am looking for tsa coating breakdown factor to use for the anode requirement calculation.


currently working a tsa with anode system!!

 
Replies continue below

Recommended for you

If you are using DNV-RP-B401, then by the definition of 'coating breakdown factor', it is 1. You are given the current densities to work with in sub-subclause 6.3.11.

Steve Jones
Materials & Corrosion Engineer

 
Hi Jones,

Thanks for the information.

Just need to clarify this coating breakdown factor , is this 1 is the initial value or the mean value .

 
is there any calculation for the thickness of tsa coating requirement available!!
 