Sep 14, 2012 #1 hsemus Petroleum Joined Apr 26, 2012 Messages 42 Location GB I am looking for tsa coating breakdown factor to use for the anode requirement calculation. currently working a tsa with anode system!!
I am looking for tsa coating breakdown factor to use for the anode requirement calculation. currently working a tsa with anode system!!
Sep 15, 2012 1 #2 SJones Petroleum Joined Apr 22, 2001 Messages 3,951 Location GB If you are using DNV-RP-B401, then by the definition of 'coating breakdown factor', it is 1. You are given the current densities to work with in sub-subclause 6.3.11. Steve Jones Materials & Corrosion Engineer http://www.linkedin.com/pub/8/83b/b04 Upvote 0 Downvote
If you are using DNV-RP-B401, then by the definition of 'coating breakdown factor', it is 1. You are given the current densities to work with in sub-subclause 6.3.11. Steve Jones Materials & Corrosion Engineer http://www.linkedin.com/pub/8/83b/b04
Sep 15, 2012 Thread starter #3 hsemus Petroleum Joined Apr 26, 2012 Messages 42 Location GB Hi Jones, Thanks for the information. Just need to clarify this coating breakdown factor , is this 1 is the initial value or the mean value . Upvote 0 Downvote
Hi Jones, Thanks for the information. Just need to clarify this coating breakdown factor , is this 1 is the initial value or the mean value .
Sep 15, 2012 Thread starter #4 hsemus Petroleum Joined Apr 26, 2012 Messages 42 Location GB is there any calculation for the thickness of tsa coating requirement available!! Upvote 0 Downvote