Hello,

We're currently working in this order to supply 50 MOVs to a gas production company, their min temperature is -50°F, our valves are from PBV and we've already asked them, however i haven't found any information regarding the temperature range for the 17-4 PH steel, i'd would like to know if this 17-4 PH stem could work correctly at these temperatures.
 
What is your specified heat treatment condition for the 17-4PH? Also, more important, what minimum CVN value at -50 deg F do you need to meet?
 
Overage material to get some reverted austenite to improve impact properties at low temperature. In terms of strength, -50F will make material stronger, while keep the same ductility.
 
Hi You may find some information on impact properties of 17-4 pH steel in the following data sheet. However the data is for bars, which are forged products. Valves involves a lot of casting, hence the mechanical properties may fluctuate widely. One has to be very careful about selection and getting the components conforming to good impact values at -50 Deg F. Also note any welding on 17-4 steel could be highly problematic
Duplex 2205 may be another material to consider.

Thanks.


Pradip Goswami,P.Eng.IWE
Welding & Metallurgical Specialist
ca.linkedin.com/pub/pradip-goswami/5/985/299
 
Why bother using 17-4PH for a valve stem. I would use Nitronic 50 and be done with it. This is material typical for valve stems.
 
Just got answer from mfg and the stem is going to be ASTM A564 GR 630 H1150D, 25 ft-lbs min avg for 3 specimens on CVN at -75F

 
This should be acceptable for the valve stem application.
 