Hi, I'm a piping engineer, It is the first time I have to work with a trisodium phosphate service, I have an issue regarding the choosing of piping material.

Does anybody have an idea of which piping material could be used?

The TSP will be disolved in condensate (water)

Thanks in advance
 
What temperature and pressure?

Want to know the do's and don'ts of Eng-Tips? Read FAQ731-376.
English not your native language? Looking for some help in getting your question across to others or understanding their answers? Go to forum1529.
 
What is the TSP concentration?

Good luck,
Latexman

Need help writing a question or understanding a reply? forum1529
 
Don't you love playing 20 questions?

Want to know the do's and don'ts of Eng-Tips? Read FAQ731-376.
English not your native language? Looking for some help in getting your question across to others or understanding their answers? Go to forum1529.
 
Creo que el inglés es una lengua segunda. Hay dificultad para expresar los detalles.

Good luck,
Latexman

Need help writing a question or understanding a reply? forum1529
 
Sorry, I meant to say, I think that English is a second language. There is difficulty to express details.

Good luck,
Latexman

Need help writing a question or understanding a reply? forum1529
 
P&T conditions are: 30°C and 38.97 kg/cm2

The TSP concentration will be 0.25kg/day in a 900litres of condensate tank.Very diluted

Thanks you all!
 
The end use of the TSP may influence the choice. What is the TSP going to clean? For example, if it is for cleaning food processing equipment, it may have to meet applicable food standards too.

Good luck,
Latexman

Need help writing a question or understanding a reply? forum1529
 
The TSP will be used as inhibitor antifouling in a boiler.
 
Then carbon steel would be just fine.

Good luck,
Latexman