Mg-alloy plate was fastened to Al 380 plate by Zn-plated steel bolt without washer. The above system was subjected to SAE J2334 corrosion test. After approximately 25 cycles I noticed signs of corrosion on the aluminum side instead of Mg-alloy.
I was told that this phenomenon is due to transpassive effect…
Since I'm not a guru in corrosion field I would like to know the nature of this effect.