Need torque value (ft-lbs) for type 316 stainless M24 bolt / nut joint, at 60% yield with anti-seize on threads.
Assumed fastener yield at 50ksi thus 30ksi when tight. Tensile area is 352.5mm^2
Oiled value came out to 276ft-lb (using 1" bolt)
NASA spec for 316 with dry lube is 155ft-lb, but I believe they use the K value for moly in that
I'm still searching for my reference charts, so any help would be appreciated!