Hi Experts!
I am designing a pressure vessel using PV Elite software which generated this report
post_kqelsk.jpg

Kindly help me understand following things:
a) Is it mandatory to consider tolerance in cyclindrical shell thickness as per div 1?
b) From where this “tu” equation is taken? I don’t find it in div 1 or I am missing something.
c) What is “tn, min” when “tn” is provided and from where this equation is taken?

Thanks in advance
 
You need to know this if you are designing pressure vessels. Are you qualified per App. 47?
 
david339933
Thanks for your reply, practicing to design in future.
 
If Ca = 0.125" and Tol% = 87.5%:
Lets say I need 0.197" (t) wall after corrosion, then I need 0.322" before corrosion (t+Ca), so I need to order 0.368" or larger (t_n,min). I order 0.375" (t_n) so I am sure to receive at least 0.328" (t_n * Tol%) which would then corrode at worst to 0.203" (t_u).
 
GBTorpenhow
Thank you so much to explain it in very simple way. Can you please guide if these calculations specified in div 1 or we calculate it ourselves to get required thickness?
 
I cannot comment on if or where these are defined in Div. 1 as I am no pressure vessel design expert but these equations are a basic part of any pressure thickness design/selection method subject to both mill tolerance and corrosion allowance.
 
You are using an old 2017 edition.
This is not a game.

Regards
 
UG-16(c) addresses plate under tolerance. Generally it doesn't have to be added as most plate specs follow the 0.01 inch (0.3 mm) rule. For example see SA-20 Table A1.1 Note 1. This is why there is no under tolerance in the calculation for your SA516-70.

UG-16(d) addresses pipe under tolerance. Generally it must be added since the manufacturing under tolerance is very large. Typically 12.5%.
 
Status