Has anyone any experience in 30%Titanium /Copper Alloys(Master Alloys). I have been asked the question - how much titanium goes into solution and what does the microstructure look like? The only info i have is that the alloy is melted at 1100 degrees C using argon as a protective atmosphere.
 