These exchangers cool the main column head gas by water sea
Alfa Laval proposed 3 Titanium welded plate exchangers for this service (Compablock Titanium grade 1 plates , T=80-100 °C, 3000 ppm h2s, 1500 ppm Nh3, <10 ppm CN, 0 ppm Cl).
API 571 par 5.1.3.2 advise for hydriding risk (NACE MR175 par. 4.2.1.4 too) in hydrocarbons side.
What's your experiences about it? Is the grade 1 the best grade for this service?
We actualy use Saf 2507 tube exchanger but we have seen crevice corrosion under gasket in floating head area in sea water side.
What material do you think better?
tx Aldo Cigna
Alfa Laval proposed 3 Titanium welded plate exchangers for this service (Compablock Titanium grade 1 plates , T=80-100 °C, 3000 ppm h2s, 1500 ppm Nh3, <10 ppm CN, 0 ppm Cl).
API 571 par 5.1.3.2 advise for hydriding risk (NACE MR175 par. 4.2.1.4 too) in hydrocarbons side.
What's your experiences about it? Is the grade 1 the best grade for this service?
We actualy use Saf 2507 tube exchanger but we have seen crevice corrosion under gasket in floating head area in sea water side.
What material do you think better?