I am a contractor located in Los Angeles,where my engineer calls for a threaded rod of 7/8" dia. placed into exiting concrete footing (24" deep) and then 6" embededment into a 12"x24"24" unpinning concrete pier with a 4"x4"x.25" washer plate attached to the end(in new pier). My question is, does the threaded rod that passes thru the existing conrete footing need to be epoxied or will the uplift force resistance by the threaded rod with the 4x4 washer on the end be enough?
7/8" Thd. Rod
____|__________________
| (e) footing |
| |
|<- Epoxy? |
____|_________________|
| | |
| | |
| _|_ |
| | |
| |
| |
|
unpinning |
| concrete |
|_____________________|
7/8" Thd. Rod
____|__________________
| (e) footing |
| |
|<- Epoxy? |
____|_________________|
| | |
| | |
| _|_ |
| | |
| |
| |
|

| concrete |
|_____________________|