Feb 4, 2009 #1 WeldGk Materials Joined Aug 14, 2007 Messages 42 Location CA Does a change from Thoriated Tungsten Electrode to Lanthanated Tungsten Electrode require requalification of WPS?
Does a change from Thoriated Tungsten Electrode to Lanthanated Tungsten Electrode require requalification of WPS?
Feb 4, 2009 #2 Mr168 Materials Joined Aug 5, 2008 Messages 731 Location US Per ASME IX QW-256, it is a non-essential variable, so no. Upvote 0 Downvote
Feb 4, 2009 #3 DVWE Petroleum Joined Apr 5, 2007 Messages 2,374 Location US If ASME IX is the code in question, then Mr168 is correct. AWS D1.1 has me scratching my head??? I believe they need to separate filler metal and electrode. I don't think it should be an essential in D1.1 either, but that's just me. Upvote 0 Downvote
If ASME IX is the code in question, then Mr168 is correct. AWS D1.1 has me scratching my head??? I believe they need to separate filler metal and electrode. I don't think it should be an essential in D1.1 either, but that's just me.