Hi all,

we have some ACM cut off machines running in our shop ( The company stopped a while ago and we had a steady supply for cutoff wheels (resinoid type abrasive). The cut off wheels measured: 4'' with a hole of 0.5'' and a thickness of 0.002''.
I remember there were suppliers in Idaho, USA who could offer these. In europe the prices are ridiculous.

Any experiences with thin resinoid cut off wheels and where to get them?

Thanks!

Sam
 
very doubtful about the thickness being .002"
 
We use Avery wheels. they are a great supplier.

= = = = = = = = = = = = = = = = = = = =
P.E. Metallurgy, Plymouth Tube
 