CREERAAM
Mechanical
- Feb 23, 2015
- 109
Dear EXPERTS,
Good Morning,
we were Mistakenly Pre Insulated the CS PIPE(ASTM A 53 Gr.B ERW)of 12 Inch SCH STD Pipe Instead of Doing 12 Inch SCH 40 Pipe. So Can i Have the option to apply the Thickness Tolerance Here to meet the SCH STD Pipe to SCH SCH 40.
NOTE : Customer Required SCH 40 Pipe Only.
SIZE OD 323.9MM Thickness SCH STD = 9.53 mm and SCH 40 = 10.31 mm.
Thanks in Advance.
REGARDS,
G.SRIRAM.
Dream,Dream,Dream Dream transforms in to thoughts.And thoughts result in action
Good Morning,
we were Mistakenly Pre Insulated the CS PIPE(ASTM A 53 Gr.B ERW)of 12 Inch SCH STD Pipe Instead of Doing 12 Inch SCH 40 Pipe. So Can i Have the option to apply the Thickness Tolerance Here to meet the SCH STD Pipe to SCH SCH 40.
NOTE : Customer Required SCH 40 Pipe Only.
SIZE OD 323.9MM Thickness SCH STD = 9.53 mm and SCH 40 = 10.31 mm.
Thanks in Advance.
REGARDS,
G.SRIRAM.
Dream,Dream,Dream Dream transforms in to thoughts.And thoughts result in action