Hi all,
I have vendor PQR's and WPS's for review . The construction code is ASME Sec 8 Div 1. In one impact tested PQR, thickness of the plate is 8 mm and the thickness range of the WPS prepared from this PQR is 8mm-16mm.But as I remember, regarding ASME B31.3 if impact tested, the qualification thickness is t/2 - t+6 mm.
Is it so for ASME Sec 8 or do I have to use ASME Sec IX?
I do not have ASME Sec 8 code for review so could you please send the reference numbers & tables in ASME Sec 8 Div 1?
Regards
Kaan
I have vendor PQR's and WPS's for review . The construction code is ASME Sec 8 Div 1. In one impact tested PQR, thickness of the plate is 8 mm and the thickness range of the WPS prepared from this PQR is 8mm-16mm.But as I remember, regarding ASME B31.3 if impact tested, the qualification thickness is t/2 - t+6 mm.
Is it so for ASME Sec 8 or do I have to use ASME Sec IX?
I do not have ASME Sec 8 code for review so could you please send the reference numbers & tables in ASME Sec 8 Div 1?