The footing slab of the 40-ft underground concrete tank I am working on will need to withstand uplift pressure (almost 35'). It does act as a ballast. Can I do 90' x60' x 12' thick slab in one pour with no joints assuming the contractor can do it..?
ACI 224 talks about 24 to 36 times the slab thickness for control joints but does not address thick slabs beyond 10”. Any recommendations to reduce the heat during placement or just use ice..?
Thank you.
ACI 224 talks about 24 to 36 times the slab thickness for control joints but does not address thick slabs beyond 10”. Any recommendations to reduce the heat during placement or just use ice..?