I have manufacture an thermowell under Nace mr103 but I dont understand this standard.
The thermowell will be in AISI 316 but I don´t Know which care I have for this.
anyone AISI316 or 316L is compliant????

Thanks in advance
 
MR0103 addresses austenitic stainless steels with carbon content up to 0.1 mass%. Therefore, both 316L and 316 are addressed under the requirements of 2.5.1

Steve Jones
Materials & Corrosion Engineer
 