Continue to Site

Eng-Tips is the largest engineering community on the Internet

Intelligent Work Forums for Engineering Professionals

  • Congratulations waross on being selected by the Eng-Tips community for having the most helpful posts in the forums last week. Way to Go!

Thermocouple adhesive

Status
Not open for further replies.

adriangillitt

Marine/Ocean
Jun 17, 2003
10
I am trying to find an adhesive to attach a thermocouple to a GRP plate. I was considering sodium silicate adhesive which can hold at high temperatures but is not very flexible, which is a problem as the plate will be flexing. I've heard that mixing this with ball clay can produce a flexible adhesive which will hold at high temperatures. Has anyone tried this or any other method for a similar application.
 
Replies continue below

Recommended for you

Ceramic will do, but why not welding a clip to to hod it?
ER










 
Look at using either epoxy or the same resin that the FRP is made from.

Cheers

Steve
 