The port I work for has been installing 175 crane rails and welding them togheter with thermite. Unfortunatly there seems to be about a 75% falure rate in those welds and were uncrtain that the ones that passed arent just going to fail in a year or two. We did ultrasonic testing on them but the tests seemed inconclusive as welds that passed UT testing failed a few days later. Dose anyone know:
1) If thermite welding is even an acceptable process for such a large rail
2) Any common reasons that the welds would have such a high falure rate
3) A better testing alternative to ut testing.
1) If thermite welding is even an acceptable process for such a large rail
2) Any common reasons that the welds would have such a high falure rate
3) A better testing alternative to ut testing.