Tek-Tips is the largest IT community on the Internet today!

Members share and learn making Tek-Tips Forums the best source of peer-reviewed technical information on the Internet!

  • Congratulations TugboatEng on being selected by the Eng-Tips community for having the most helpful posts in the forums last week. Way to Go!

Thermal staking parameters

Status
Not open for further replies.

ankith32

Mechanical
Joined
Nov 27, 2011
Messages
2
I'm trying to heat stake bracket made from nylon-6. I'm having trouble finding any ball park figures for the pressure applied or the temperature of the die.
 
It's pretty much trial and error, however nylons melt suddenly at quite high temperatures.

They also absorb moisture from the atmosphere over time. If wet when heated to melting point the out gas water vapour ans spit and sizzle.

I would think about 220 to 240 deg C and very light pressure, probably toward the minimum setting on the machine.

Regards
Pat