Dear Sirs,
Is Thermal Stability required more than 150 minutes for a HDPE Pipe at 200 Deg.C? ASTM D 3895 - 07 mentioned Oxidatin Induction Time (OIT) for HDPE material / pipe is more than 150 minutes at 200 Deg.C, Whereas all other internaltional standards ISO 4427, EN 12232 etc, giving OIT for HDPE shall be > 20 min at 200 Deg.C is sufficient. We are under impression & according to information from sources, that the value mentioned in ASTM have a typographic error, is it correct? or it's really required that many minutes of thermal stability? Any one can explain in detail? Thanks in advance - RAM
Is Thermal Stability required more than 150 minutes for a HDPE Pipe at 200 Deg.C? ASTM D 3895 - 07 mentioned Oxidatin Induction Time (OIT) for HDPE material / pipe is more than 150 minutes at 200 Deg.C, Whereas all other internaltional standards ISO 4427, EN 12232 etc, giving OIT for HDPE shall be > 20 min at 200 Deg.C is sufficient. We are under impression & according to information from sources, that the value mentioned in ASTM have a typographic error, is it correct? or it's really required that many minutes of thermal stability? Any one can explain in detail? Thanks in advance - RAM