Dear ALL,

I NEED A INPUT TO CALCULATE THE DISPLACEMENT OF THE PUMP NOZZLE, THE MOC OF THE PUMP CASING IS ASTM A 995 GR 5A, WHICH I AM NOT ABLE TO FIND IN STANDARDS,
IF ANYONE CAN HELP IN GETTING THE SUBJECT DETAILS FOR (TEMP: 9, 21, 85 DEG CELCIUS) WOULD BE HELPFUL.

THANKS
IRANNA
 
I don't know if you will find a CTE for the cast version, you could start using the wrought equivalent though, S32750.

= = = = = = = = = = = = = = = = = = = =
P.E. Metallurgy, consulting work welcomed
 
Yeah, just use data for the nearest alloy that is similar in overall composition.
Then turn off your caps lock.

"Everyone is entitled to their own opinions, but they are not entitled to their own facts."
 