HI fRIENDS,I need your technical advice.
I have an ASME SECTION VIII DIV-2 VESSEL in which the internal ladder rungs are to be welded below the manhole to reach to the base of the vessel.
It is 60 mm thick vessel with internal ladder rungs .
THE VESEL PWHT AND HYDRO TEST COMPLETED .Manufacturer forgot to weld this ladder rungs inside the vessel below the Manhole before doing the PWHT and Hydro test.
Can I weld the ladder rungs to the shell internal using a fillet weld after completing this PWHT/Hydro test?
Does it requires PWHT after welding this ladder rungs to shell?
Do I need to rehydrotest the vessel along with these ladder rungs after PWHT ?
What the technical things to be follwed if I want to weld these ladder rungs to the already PWHT/Hydrotested vessel?
This vessel is in mild sour service with 7 PPM H2S service.
Advice is highly apprciated ASAP as we are holding the box up of this vessel in construction site
Regards,
Saji Panakakttil
I have an ASME SECTION VIII DIV-2 VESSEL in which the internal ladder rungs are to be welded below the manhole to reach to the base of the vessel.
It is 60 mm thick vessel with internal ladder rungs .
THE VESEL PWHT AND HYDRO TEST COMPLETED .Manufacturer forgot to weld this ladder rungs inside the vessel below the Manhole before doing the PWHT and Hydro test.
Can I weld the ladder rungs to the shell internal using a fillet weld after completing this PWHT/Hydro test?
Does it requires PWHT after welding this ladder rungs to shell?
Do I need to rehydrotest the vessel along with these ladder rungs after PWHT ?
What the technical things to be follwed if I want to weld these ladder rungs to the already PWHT/Hydrotested vessel?
This vessel is in mild sour service with 7 PPM H2S service.
Advice is highly apprciated ASAP as we are holding the box up of this vessel in construction site
Regards,
Saji Panakakttil