The S31254 super stainless steel plate was subjected to a welding process procedure experiment, with bending fracture

yellos

Mechanical
Joined
Jul 23, 2025
Messages
1
Recently, I have been working on the welding process program for S31254, featuring 10mm sheet material, GTAW, 99.99%Ar protection, current of 110A, and filler material ERNiCrMo-3. The test results show that the tensile test is qualified while the bending test breaks. May I ask what the reason is?
 

Attachments

  • 微信图片_20250723100401.jpg
    微信图片_20250723100401.jpg
    140.5 KB · Views: 8
The reason is most likely found in your materials failure analysis report
 
How many weld passes?
What inspection between passes?
Control of interpass temperature?
Sounds like a weld procedure issue to me.
254 is straightforward to weld and there is a lot of information out there.
 