The lithium bromide used in absorption chillers is corrosive to steel. It usually has an inhibitor such as lithium nitrate or lithium chromate mixed with it to control corrosion, but in general, the lithium bromide could be expected to enhance the corrosion of rebar in concrete in a manner similar to chlorides.